Honestly, I use just one, Bondo Spot and Glasing Putty, and it's only for minor or thin fills.

The rest, I use good old plastic and super glue. It dries hard, stays stable, doesn't shrink and can be worked the same as the rest of the plastic kit. And it's fast - no long waiting. 

Other builders may disagree, but I've had bad, long term experiences with all kinds of fillers shrinking and cracking.

I also try to plan my cuts carefully and prep parts to fit precisely and neatly, to minimize sloppy puttying. Think of what were doing as miniature "Overhaulin' " shops. Look at how neat and clean their cars are BEFORE they ever put any paint on them. A final finish is only as good as it's foundation.

Besides, if something happens (God forbid) and you have to strip the paint off,  you won't have as much to re-putty again later.

Just my way of doing it.

Link to comment
Share on other sites

34 minutes ago, Oldcarfan27 said:

Besides, if something happens (God forbid) and you have to strip the paint off,  you won't have as much to re-putty again later.

That's why I use Magic-Sculpt. It's impervious to all stripping chemicals/solvents and, being a two-part epoxy, doesn't shrink or crack. Reshaped RoG Ferrari 250 GTO rear end using this stuff.

IMG_4476aa.jpg.3dfb7c2ee4f3d129b323ffaaeb0ea4c1.jpg

IMG_4474a.jpg.84bb1156f7864aef2f40e69f114390e7.jpg

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.
Note: Your post will require moderator approval before it will be visible.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...